Yasufumi WatanabeYuji ShibasakiShinji AndoMitsuru Ueda
Abstract We prepared new semiaromatic polyimides from alicyclic dianhydrides and aromatic diamines containing adamantyl and biadamantyl units. Polycondensations were performed in 1‐methyl‐2‐pyrrolidinone at room temperature for 7 h and then 80 °C for 23 h, giving poly(amic acid)s with inherent viscosities up to 0.58 dL/g. Poly(amic acid)s were converted to corresponding poly(imide)s by thermal treatment. Poly(imide)s showed relatively high thermal stability (5% weight loss around 450 °C) and low dielectric constants (2.69–2.79). © 2003 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 42: 144–150, 2004