Abstract Natural rubber compound with different blend ratios of sulfur was prepared. Fabrication of shape memory polymer by swelling natural rubber compound with palmitic acid at 75 °C (100 wt% palmitic acid loading). Shape recovery experiments run by stretching to 100% (1 hour) at permanent set after heating treatment in a water bath (75°C for 30 s) and then freezing in 10°C water for 30 s. The samples were subsequently reheated in a water bath to recover the permanent shape (three stretching cycles). Shape memory compound swollen palmitic acid exhibited shape recovery of 96-100% and shape fixity 57-98%. Repeated shape recovery cycles had little effect on its shape memory property and mechanical property.