JOURNAL ARTICLE

PLA Nanofibers Electrospun from System of Low Toxicity Solvent

Li Wei LiuWeimin KangBowen ChengYa Liu

Year: 2011 Journal:   Advanced materials research Vol: 221 Pages: 657-661   Publisher: Trans Tech Publications

Abstract

In this paper polylactide (PLA) nanofibers were successfully prepared via electrospinning using low toxic 1,4-dioxane and acetone as co-solvents. The morphology of nanofibers was studied by scanning electron microscopy (SEM) at the different weight ratios of co-solvent, concentrations of spinning solution, electrostatic voltages and collecting distance. Results indicate that the finer and uniform nanofibers were electrospun from the concentration of the spinning solutions at 8 wt.%, 1,4-dioxane and acetone with ratio of 40/60 (w/w), the spinning voltage at 20kV, the collecting distance at 180 mm and the extruding speed at 5 mL/h.

Keywords:
Nanofiber Electrospinning Acetone Spinning Solvent Scanning electron microscope Materials science Chemical engineering Morphology (biology) Composite material Polymer chemistry Chemistry Polymer Organic chemistry

Metrics

1
Cited By
0.00
FWCI (Field Weighted Citation Impact)
12
Refs
0.11
Citation Normalized Percentile
Is in top 1%
Is in top 10%

Citation History

Topics

Electrospun Nanofibers in Biomedical Applications
Physical Sciences →  Materials Science →  Biomaterials
Advanced Sensor and Energy Harvesting Materials
Physical Sciences →  Engineering →  Biomedical Engineering
biodegradable polymer synthesis and properties
Physical Sciences →  Materials Science →  Biomaterials