Yanfu LinYujin ChenHaomiao ZhuXinghong GongZundu LuoYidong Huang
An Yb3+ : YAl3(BO3)4/YAl3(BO3)4 composite is obtained by the segmented crystal growth method. Diode-pumped laser operation is demonstrated in the 2.0 mm thick, (0 0 1)-oriented composite with a 0.8 mm thick, 9.5 at% Yb3+ : YAl3(BO3)4 crystal segment. Under the absorbed pump power of 11.9 W, quasi-continuous-wave output powers of 0.82 W with a slope efficiency of nearly 20% and of 0.3 W with a slope efficiency of 10.5% around 1040 nm are achieved in hemispherical and plano–plano cavities, respectively.
李渊骥 Li Yuanji焦月春 Jiao Yuechun冯晋霞 Feng Jinxia张宽收 Zhang Kuanshou陈雨金 Chen Yujin林炎富 Lin Yanfu黄艺东 Huang Yidong
Д. А. НапрасниковВ. В. МальцевН. И. Леонюк
肖林久 XIAO Lin-jiu刘娇娜 LIU Jiao-na谢颖 XIE Ying王刚 WANG Gang陈永杰 CHEN Yong-jie李文泽 LI Wen-ze耿秀娟 GENG Xiu-juan
Hisashi YoshidaKazuhiro FujikawaHiroaki ToyoshimaShinta WatanabeKazuyoshi Ogasawara
R. Satheesh KumarV. PonnusamyM.T. JoseV. Sivakumar