Wencai ZhouXiujie HuXiaoxia BaiShuyun ZhouChenghua SunJun YanPing Chen
Highly regulated core-shell Fe(3)O(4)-poly(3, 4-ethylenedioxythiophene) (PEDOT) microspheres were successfully synthesized by a two-step method in the presence of polyvinyl alcohol (PVA) and p-toluenesulfonic acid (p-TSA). And their morphology, microstructure, electromagnetic and microwave absorbing properties were subsequently characterized. By simply adjusting the molar ratio of 3, 4-ethylenedioxythiophene (EDOT) to Fe(3)O(4) (represented by (EDOT)/(Fe(3)O(4))), the thickness of the polymer shell can be tuned from tens to hundreds of nanometers. Moreover, it was found that the composite exhibited excellent microwave absorbing property with a minimum reflection loss (RL) of about -30 dB at 9.5 GHz with a (EDOT)/(Fe(3)O(4)) ratio of 20.
Wencai ZhouXiujie HuChenghua SunJun YanShuyun ZhouPing Chen
Yujin ChenGang XiaoTieshi WangQiuyun OuyangLihong QiYang MaPeng GaoChunling ZhuMao‐Sheng CaoHaibo Jin
Yujin ChenPeng GaoRuixuan WangChunling ZhuLijiao WangMao‐Sheng CaoHaibo Jin
Jing ZhaoJunpin LinJunping XiaoHuili Fan
Manuel RamosKarina CastilloD. FerrerRurik FaríasS. FloresRussell R. Chianelli